Finding lubricants that work at exceptionally high temperatures challenges researchers and industries alike. Recently, a Virginia Tech team may have uncovered a promising candidate by happenstance: transition metal spinel oxides formed on nickel…
Finding lubricants that work at exceptionally high temperatures challenges researchers and industries alike. Recently, a Virginia Tech team may have uncovered a promising candidate by happenstance: transition metal spinel oxides formed on nickel… Finding lubricants that work at exceptionally high temperatures challenges researchers and industries alike. Recently, a Virginia Tech team may have uncovered a promising candidate by happenstance: transition metal spinel oxides formed on nickel…